This article describes various evaluation techniques of fractography such as visual inspection, macroscopic and microscopic examinations that are used to resolve different aspects of failure. It gives a brief description and pictorial representation of various defects leading to fracture of metals, including laps, seams, cold shuts, cracks, inclusions, porosity, fatigue, and stress corrosion cracking.

You do not currently have access to this content.
Don't already have an account? Register

1998. "Use of Fractography for Failure Analysis", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal