Abstract

Alloys based on ordered intermetallic compounds constitute a unique class of metallic material that form long-range ordered crystal structures below a critical temperature. Aluminides, a unique class of ordered intermetallic materials, possesses many attributes like low densities, high melting points, and good high-temperature strength that make them an attractive material for high-temperature structural application. This article discusses the properties, chemical composition, corrosion resistance, processing, fabrication, alloying effects and crystallographic data of nickel aluminides (Ni3Al and NiAl), iron aluminides (Fe3Al and FeAl) and titanium aluminides (alpha-2 alloys, orthorhombic alloys, and gamma alloys).

You do not currently have access to this content.
Don't already have an account? Register

1998. "Structural Intermetallics", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal