Processing of Titanium and Titanium Alloys

By
Rodney R. Boyer
Rodney R. Boyer
Editing author
Boeing Commercial Airplane Company
Search for other works by this author on:
Published:
1998
Page range:
578 - 584

Abstract

Titanium metal passes through three major steps during processing from ore to finished product: reduction of titanium ore to sponge (porous form), melting of sponge and scrap to form ingot, and remelting and casting into finished shape. This Article describes primary fabrication, including all operations that convert ingot into general mill products, such as billet, bar, plate, sheet, strip, tube, and wire. The section on secondary fabrication describes processes such as die forging, extrusion, hot and cold forming, machining, chemical milling, and joining. The Article presents a short note on powder metallurgy products of titanium. Casting processes and properties are covered in the final section.

You do not currently have access to this content.
Don't already have an account? Register

Rodney R. Boyer, 1998. "Processing of Titanium and Titanium Alloys", Metals Handbook Desk Edition, Joseph R. Davis