Alloy and Temper Designation Systems for Aluminum

Published:
1998
Page range:
423 - 426

Abstract

This article describes the systems for designating the aluminum and aluminum alloys that incorporate the product forms (wrought, casting or foundry ingots) and its respective temper for strain-hardened alloys, heat-treatable alloys and annealed alloys. All these systems are covered by American National Standards Institute (ANSI) standard H35.1. Furthermore, the article provides a short note on the designation of unregistered tempers.

You do not currently have access to this content.
Don't already have an account? Register

1998. "Alloy and Temper Designation Systems for Aluminum", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal