Magnetically Soft Materials

Published:
1998
Page range:
639 - 644

Abstract

This article discusses the ferromagnetic properties of soft magnetic materials, and explains the effects of impurities, alloying elements, heat treatment, grain size, and grain orientation on soft magnetic materials. It describes the types of soft magnetic materials, which include high-purity iron, low-carbon irons, silicon (electrical) steels, nickel-iron alloys, iron-cobalt alloys, ferritic stainless steels, amorphous metals, and ferrites (ceramics). Finally, the article provides information on the alloys for magnetic temperature compensation.

You do not currently have access to this content.
Don't already have an account? Register

1998. "Magnetically Soft Materials", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal