Stainless steel powder metallurgy (P/M) parts represent an important and growing segment of the P/M industry. This article describes the processing, properties, and composition of medium-density and high-density P/M stainless steels. Medium-density materials are processed by pressing and sintering prealloyed stainless powders. High-density materials are produced by hot isostatic pressing, cold isostatic pressing followed by extrusion, or metal injection molding. The comparison of mechanical properties of these P/M stainless steels is represented graphically. The article contains a table that lists the effect of iron, carbon, nitrogen, oxygen, and density on the corrosion resistance of the sintered austenitic stainless steels.

You do not currently have access to this content.
Don't already have an account? Register

1998. "P/M Stainless Steels", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal