Glossary of Terms

Published:
1995
Page range:
3 - 72

Abstract

This article is a compilation of definitions for terms related to engineering materials, including plastics, elastomers, polymer-matrix composites, adhesives and sealants, ceramics, ceramic-matrix composites, glasses, and carbon-carbon composites.

You do not currently have access to this content.
Don't already have an account? Register

1995. "Glossary of Terms", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier