Elastomers

By
Rebecca Tuszynski
Rebecca Tuszynski
Search for other works by this author on:
Published:
1995
Page range:
282 - 286

Abstract

This Article discusses the properties, chemical structures, and applications of different types of elastomers grouped based on their resistance to aging (oxidative degradation), solvents, and temperature. These include butadiene rubber, natural rubber, isoprene rubber, chloroprene rubber, styrene-butadiene rubber, aerylonitrile-butadiene (nitrile) rubber, isobutylene-isoprene (butyl) rubber, ethylene-propylene (-diene) rubber, and silicone rubber. The Article also provides an outline of the concerns related to the processing stages of rubbers or elastomers, including mixing or compounding, shaping, and vulcanizing or crosslinking.

You do not currently have access to this content.
Don't already have an account? Register

Rebecca Tuszynski, 1995. "Elastomers", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal