Skip to Main Content
ASM Desk Editions

Engineered Materials Handbook Desk Edition

Edited by
Michelle M. Gauthier
Michelle M. Gauthier
Raytheon Company
Search for other works by this author on:
ASM International
ISBN electronic:
978-1-62708-200-6
Publication date:
1995
Book Chapter

Metallizing of Plastics

By
Rebecca Tuszynski
Rebecca Tuszynski
HBM Company
Search for other works by this author on:
N.V. Mandich
N.V. Mandich
HBM Company
Search for other works by this author on:
Published:
1995
Page range:
356 - 364

Abstract

The process of coating plastics with metals for functional purposes is called metallizing of plastics. This article discusses the metallizing of plastics, provides information on its history, and gives a short note on applications and adhesion properties of metallic coatings. It also discusses the selection of plastics for plating. This article also describes metallizing techniques, including plating (electrolytic or electroplating), vacuum metallizing and thermal spraying, and environmental considerations. The article discusses the quality assurance procedures for metallized plastic parts which include tests that assess the quality of the finish, coating thickness, adhesion, and corrosion resistance, and gives a short note on service performance, which includes service condition classifications.

You do not currently have access to this content.
Don't already have an account? Register

Rebecca Tuszynski, N.V. Mandich, 1995. "Metallizing of Plastics", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal