Electrical Testing of Polymers

Published:
1995
Page range:
423 - 438

Abstract

In terms of their electrical properties, plastics can be divided into thermosetting and thermoplastic materials, some of which are conductive or semiconductive. This article provides detailed information on factors that affect the property of plastics. It discusses the major test methods used to determine the following dielectric properties of plastics: dielectric breakdown voltage, dielectric strength, dielectric constant, dissipation factor, arc tracking resistance, insulation resistance, volume, and surface resistivity or conductivity. The test specifications and conditions, recommended by several U.S. and foreign testing organizations for characterizing the electrical properties of plastic materials are listed. The article describes the influence of these properties on selection of plastics for insulation application. An outline of the electromagnetic shielding and testing methods of electromagnetic interference are also provided. Designations, electrical properties, and applications of elastomers are tabulated.

You do not currently have access to this content.
Don't already have an account? Register

1995. "Electrical Testing of Polymers", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal