Resin Transfer Molding and Structural Reaction Injection Molding

Published:
1995
Page range:
336 - 341

Abstract

Resin transfer molding (RTM) and structural reaction injection molding (SRIM) are two similar processes that are well suited to the manufacture of large, complex, and high-performance structures. This article discusses the similarities and differences of RTM and SRIM processes and the unique design considerations with respect to the physical properties, geometry, surface quality, process economics, equipment, and tooling of a component that should be considered in choosing RTM or SRIM over other competing processes for fabricating reinforced components.

You do not currently have access to this content.
Don't already have an account? Register

1995. "Resin Transfer Molding and Structural Reaction Injection Molding", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal