Honeycomb

Published:
1995
Page range:
546 - 550

Abstract

Honeycomb is a product consisting of very thin sheets attached to form connecting cells. This article briefly explains the construction, core characteristics, properties, and testing methods of the honeycomb structures. It discusses the special processes used to custom fit the shape of core to fit customer’s specific needs. The article provides information on sandwich structures, including material selection, design guidelines, and structural efficiency.

You do not currently have access to this content.
Don't already have an account? Register

1995. "Honeycomb", Engineered Materials Handbook Desk Edition, Michelle M. Gauthier

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal