Book Chapter

Analysis of Creep and Creep-Rupture Data[1],[2]

By
M.K. Booker
M.K. Booker
Oak Ridge National Laboratory
Search for other works by this author on:
Published:
2000
Publication history
May 20, 2015

Abstract

This article presents typical problems encountered in the analysis of experimental creep and creep-rupture data and the possible solutions to these drawbacks. It provides information on planning the test and creep strain/time relationships. The exponential creep equation and the rational polynomial creep equation are discussed. The article also describes the dependence of stress and temperature on equation parameters and explains the lot-centered regression analysis.

You do not currently have access to this content.
Don't already have an account? Register

M.K. Booker, 2000. "Analysis of Creep and Creep-Rupture Data,", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal