Design Allowables for Static Metallic Material Properties[1]

By
Paul E. Ruff
Paul E. Ruff
Battelle Columbus Laboratories
Search for other works by this author on:
Published:
2000
Publication history
May 20, 2015

Abstract

Statistical analysis of mechanical property data is the most reliable method for determination of minimum design allowables. This article describes the general procedures used to determine design allowables. It provides information on the determination of a distribution form. The article presents statistical methods which help in determining design allowables. These methods include direct computation for normal distribution, direct computation for an unknown distribution, computation of derived properties, and regression analysis. The article concludes with information on low- and elevated-temperature design properties.

You do not currently have access to this content.
Don't already have an account? Register

Paul E. Ruff, 2000. "Design Allowables for Static Metallic Material Properties", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal