Skip to Main Content
ASM Handbook

Mechanical Testing and Evaluation

Edited by
Howard Kuhn
Howard Kuhn
Search for other works by this author on:
Dana Medlin
Dana Medlin
Search for other works by this author on:
ASM International
Volume
8
ISBN electronic:
978-1-62708-176-4
Publication date:
2000
Book Chapter

Mechanical Behavior Under Tensile and Compressive Loads[1]

By
George E. Dieter
George E. Dieter
University of Maryland
Search for other works by this author on:
Published:
2000
Page range:
99 - 108

Abstract

This article focuses on mechanical behavior of materials under conditions of uniaxial tension and compression. The emphasis is on mechanical behavior during the engineering tension test, which is used to provide basic design information on the strength of materials and as an acceptance test for the specification of materials. The article presents mathematical expressions for a flow curve of many metals in the region of uniform plastic deformation. It explains that the rate at which strain is applied to the tension specimen has an important influence on the stress-strain curve. The point of necking at maximum load can be obtained from the true stress-true strain curve by finding the point on the curve having a subtangent of unity. The article concludes with an overview of the ductility measurements performed by notch tensile and compression tests.

You do not currently have access to this content.
Don't already have an account? Register

George E. Dieter, 2000. "Mechanical Behavior Under Tensile and Compressive Loads", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal