Testing of Adhesive Joints

By
K.L. DeVries
K.L. DeVries
University of Utah
Search for other works by this author on:
Paul Borgmeier
Paul Borgmeier
University of Utah
Search for other works by this author on:
Published:
2000
Page range:
836 - 844

Abstract

Adhesive joints involve joining parts by bonding component parts together with an adhesive. This article provides a discussion on the purpose of testing adhesive joints and on the factors influencing mechanical strength of these joints. It describes the various tests used in the measurement of adhesive joint strength. These include qualitative tests, peel tests, lap shear tests, tensile tests, and adhesive fracture mechanics tests.

You do not currently have access to this content.
Don't already have an account? Register

K.L. DeVries, Paul Borgmeier, 2000. "Testing of Adhesive Joints", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin