Skip to Main Content
ASM Handbook

Mechanical Testing and Evaluation

Edited by
Howard Kuhn
Howard Kuhn
Search for other works by this author on:
Dana Medlin
Dana Medlin
Search for other works by this author on:
ASM International
Volume
8
ISBN electronic:
978-1-62708-176-4
Publication date:
2000
Book Chapter

Mechanical Testing for Metalworking Processes

By
Serope Kalpakjian
Serope Kalpakjian
Illinois Institute of Technology
Search for other works by this author on:
Published:
2000
Page range:
70 - 78

Abstract

An important activity in metalworking facilities is the testing of raw materials for characteristics that ensure the integrity and quality of the products made. This article reviews the common material parameters that can have a direct or indirect influence on workability and product quality. These include strength, ductility, hardness, strain-hardening exponent, strain-rate effects, temperature effects, and hydrostatic pressure effects. The article also reviews the material behavior characteristics typically determined by mechanical testing methods. It discusses various mechanical testing methods, including the tension test, plane-strain tension test, compression test, plane-strain compression test, partial-width indentation test, and torsion test. Aspects of testing particularly relevant to workability and quality control for metalworking processes are also described. Finally, the article details the various factors influencing workability in bulk deformation processes and formability in sheet-metal forming.

You do not currently have access to this content.
Don't already have an account? Register

Serope Kalpakjian, 2000. "Mechanical Testing for Metalworking Processes", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal