Tension and Compression Testing at Low Temperatures

By
Robert P. Walsh
Robert P. Walsh
National High Magnetic Field Laboratory, Florida State University
Search for other works by this author on:
Published:
2000
Page range:
164 - 171

Abstract

This article provides a discussion on the mechanical properties of metals, ceramics, and polymers and fiber-reinforced polymer composites at low temperatures. It reviews the factors to be considered in tensile and compression testing of these materials. The article details the equipment used for low-temperature tensile and compression tests with illustrations. It concludes with a discussion on the various test methods and their ASTM standard for compression and tension testing.

You do not currently have access to this content.
Don't already have an account? Register

Robert P. Walsh, 2000. "Tension and Compression Testing at Low Temperatures", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal