Skip to Main Content
ASM Handbook

Mechanical Testing and Evaluation

Edited by
Howard Kuhn
Howard Kuhn
Search for other works by this author on:
Dana Medlin
Dana Medlin
Search for other works by this author on:
ASM International
Volume
8
ISBN electronic:
978-1-62708-176-4
Publication date:
2000
Book Chapter

Mechanical Testing of Fiber-Reinforced Composites[1]

By
Dale Wilson
Dale Wilson
The Johns Hopkins University
Search for other works by this author on:
Leif A. Carlsson
Leif A. Carlsson
Florida Atlantic University
Search for other works by this author on:
Published:
2000
Page range:
905 - 932

Abstract

This article begins with a review of the purposes of mechanical characterization tests and the general considerations related to the mechanical properties of anisotropic systems, specimen fabrication, equipment and fixturing, environmental conditioning, and analysis of test results. It provides information on the specimen preparation, instrumentation, and procedures for various mechanical test methods of fiber-reinforced composites. These include the compression test, flexure test, shear test, open hole tension test, and compression after impact test. The article describes three distinct fracture modes, namely, crack opening mode, shearing mode, and tearing mode. It presents an overview of fatigue testing and fatigue damage mechanisms of composite materials and reviews the types of mechanical measurements that can be made during the course of testing to assess fatigue damage. The article concludes with a discussion on the split-Hopkinson pressure bar test.

You do not currently have access to this content.
Don't already have an account? Register

Dale Wilson, Leif A. Carlsson, 2000. "Mechanical Testing of Fiber-Reinforced Composites", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal