Shear, Torsion, and Multiaxial Testing

By
Howard A. Kuhn
Howard A. Kuhn
Concurrent Technologies Corporation
Search for other works by this author on:
Published:
2000
Page range:
185 - 194

Abstract

This article reviews the common methods of shear and multiaxial testing for the evaluation of engineering components such as fasteners and mill products. It discusses shear test methods, including through-thickness tests, in-plane shear tests, and double-notched shear test. The article provides information on torsional (rotational shear) tests as well as the basic equipment and setup of torsion testing. Motors, twist and torque transducers, torque sensors, and heating systems as well as the specimen preparation procedure are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Howard A. Kuhn, 2000. "Shear, Torsion, and Multiaxial Testing", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal