Creep Crack Growth Testing

By
B.E. Gore
B.E. Gore
Northwestern University
Search for other works by this author on:
W. Ren
W. Ren
Air Force Materials Laboratory
Search for other works by this author on:
P.K. Liaw
P.K. Liaw
The University of Tennessee
Search for other works by this author on:
Published:
2000
Page range:
586 - 595

Abstract

Predicting the service life of structural components involves creep-fatigue crack growth (CFCG) testing under pure creep conditions. This article provides a discussion on the loading condition and the type of ductile and brittle material showing creep behavior. It focuses on a description of the experimental method that should be followed in conducting tests of CFCG with various hold times. The article describes the testing conditions, definitions, and the necessary calculations of various crack-tip parameters considered during static and cyclic loading in time-dependent fracture mechanics. The parameters considered for static loading are C*, C(t), C*(t), C*h, Ct, and Cst(t). For cyclic loading, the parameters are delta Jc and (Ct)avg. An overview of life-prediction models is also provided.

You do not currently have access to this content.
Don't already have an account? Register

B.E. Gore, W. Ren, P.K. Liaw, 2000. "Creep Crack Growth Testing", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal