Sliding Contact Damage Testing

Published:
2000
Page range:
346 - 358

Abstract

Surface damage from sliding contact is related to the adhesion of mating surfaces in contact. This article describes the methods for evaluation of surface damage caused by sliding contact. It defines adhesive wear in terms of asperity, cold welding, galling, scuffing, seizure, and wear coefficient. The article discusses various galling testing methods, such as button-on-block galling test, pin-on-flat galling test, and threaded connection galling test. It provides an overview of fretting wear that occurs between two tight-fitting surfaces subjected to a cyclic, relative motion of extremely small amplitude. The article also reviews the fretting rig for investigating fretting wear.

You do not currently have access to this content.
Don't already have an account? Register

2000. "Sliding Contact Damage Testing", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal