Stress Relaxation Testing

By
D.A. Woodford
D.A. Woodford
MPa, Inc.
Search for other works by this author on:
Published:
2000
Page range:
398 - 404

Abstract

This article discusses stress relaxation testing on metallic materials, as covered by ASTM E 328. It reviews the two types of stress relaxation tests performed in tension, long-term and accelerated testing. The article illustrates load characteristics and data representation for stress relaxation testing used for the most convenient and common uniaxial tensile test. It concludes with information on compression testing, bend testing, torsion testing, and tests on springs.

You do not currently have access to this content.
Don't already have an account? Register

D.A. Woodford, 2000. "Stress Relaxation Testing", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal