Abstract

The separation of the fatigue process into crack initiation and propagation phases has been an important and useful advance in engineering. The combined approach of strain-control testing and the development fracture mechanics of fatigue crack growth rates is a key advance that allows better understanding and simulation of both crack nucleation and the subsequent crack growth mechanisms. This article reviews three basic types of fatigue properties: stress-life, strain life, and fracture mechanic crack growth.

You do not currently have access to this content.
Don't already have an account? Register

2000. "Fatigue and Fracture Mechanics", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal