Macroindentation Hardness Testing

By
Edward L. Tobolski
Edward L. Tobolski
Wilson Instruments Division, Instron Corporation
Search for other works by this author on:
Andrew Fee
Andrew Fee
Consultant
Search for other works by this author on:
Published:
2000
Page range:
203 - 220

Abstract

This article describes the principal methods for macroindentation hardness testing by the Brinell, Vickers, and Rockwell methods. For each method, the test types and indenters, scale limitations, testing machines, calibration, indenter selection and geometry, load selection and impression size, testing methodology, and testing of specific materials are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Edward L. Tobolski, Andrew Fee, 2000. "Macroindentation Hardness Testing", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal