Skip to Main Content
ASM Handbook

Mechanical Testing and Evaluation

Edited by
Howard Kuhn
Howard Kuhn
Search for other works by this author on:
Dana Medlin
Dana Medlin
Search for other works by this author on:
ASM International
Volume
8
ISBN electronic:
978-1-62708-176-4
Publication date:
2000
Book Chapter

Introduction to the Mechanical Behavior of Metals

By
Todd M. Osman
Todd M. Osman
U.S. Steel Research
Search for other works by this author on:
Joseph D. Rigney
Joseph D. Rigney
General Electric Aircraft Engines
Search for other works by this author on:
Published:
2000
Page range:
3 - 12

Abstract

Mechanical properties are described as the relationship between forces (or stresses) acting on a material and the resistance of the material to deformation (i.e., strains) and fracture. This article briefly introduces the typical relationships between metallurgical features and the mechanical behavior of metals. It explains the deformation and fracture mechanisms of these metals. Typical properties measured during mechanical testing related to these deformation mechanisms and the microstructures of metals are discussed. The article reviews the various factors that affect the deformation response of the metal: strain rate, temperature, nature of loading, stress-corrosion cracking, and presence of notches.

You do not currently have access to this content.
Don't already have an account? Register

Todd M. Osman, Joseph D. Rigney, 2000. "Introduction to the Mechanical Behavior of Metals", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal