Hardness Conversions for Steels

Published:
2000
Page range:
282 - 287

Abstract

Hardness conversions are empirical relationships defined by conversion tables limited to specific categories of materials. This article is a collection of tables that present approximate Rockwell B hardness conversion numbers for nonaustenitic steels as per ASTM E 140 and approximate equivalent hardness numbers for the Brinell hardness and the Vickers (diamond pyramid) hardness numbers for steel.

You do not currently have access to this content.
Don't already have an account? Register

2000. "Hardness Conversions for Steels", Mechanical Testing and Evaluation, Howard Kuhn, Dana Medlin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal