Skip to Main Content
ASM Handbook

Corrosion: Fundamentals, Testing, and Protection

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter

Corrosion Resistance of Stainless Steels and Nickel Alloys

By
A. John Sedriks
A. John Sedriks
Office of Naval Research
Search for other works by this author on:
Published:
2003
Page range:
697 - 702
Publication history
December 01, 2003

Abstract

Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This article examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on corrosion resistance of these materials. It provides information on the compositions of selected stainless steels, copper-nickel, and nickel-base alloys in a tabular form. The article also illustrates the compositional and property linkages for stainless steels and nickel-base alloys.

You do not currently have access to this content.
Don't already have an account? Register

A. John Sedriks, 2003. "Corrosion Resistance of Stainless Steels and Nickel Alloys", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal