Electrochemical Methods of Corrosion Testing

By
Florian Mansfeld
Florian Mansfeld
University of Southern California
Search for other works by this author on:
Published:
2003
Page range:
446 - 462
Publication history
December 01, 2003

Abstract

This article reviews the fundamentals of electrochemical corrosion test methods. The features and requirements of the instrumentation needed for an electrochemical test are briefly discussed. The article provides a discussion on the various electrochemical techniques and tests available for laboratory studies of corrosion phenomena. The techniques and tests include no-applied-signal tests, small-signal polarization tests, large-signal polarization tests, scanning electrode techniques, and miscellaneous techniques.

You do not currently have access to this content.
Don't already have an account? Register

Florian Mansfeld, 2003. "Electrochemical Methods of Corrosion Testing", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal