Introduction to Corrosion Resistance of Bulk Materials

By
Paul Natishan
Paul Natishan
Naval Research Laboratory
Search for other works by this author on:
Published:
2003
Page range:
687 - 688
Publication history
December 01, 2003

Abstract

This article discusses factors that influence the effect of alloying, metallurgical treatments, and mechanical treatments on the corrosion resistance of metallic materials, with schematic illustrations.

You do not currently have access to this content.
Don't already have an account? Register

Paul Natishan, 2003. "Introduction to Corrosion Resistance of Bulk Materials", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.