Materials Selection for Corrosion Control

By
Peter Elliott
Peter Elliott
Revising author
Corrosion & Materials Consultancy, Inc.
Search for other works by this author on:
Published:
2003
Page range:
909 - 928
Publication history
December 01, 2003

Abstract

This article outlines the processes by which materials are selected to prevent or control localized corrosion, galvanic corrosion, and intergranular corrosion. It reviews the operating conditions and the design of candidate materials for material selection. The article discusses various corrosion-resistant materials, including ferrous and nonferrous metals and alloys, thermoplastics, reinforced thermosetting plastics, nonmetallic linings, glass, carbon and graphite, and catalyzed resin coatings. It examines an unusual form of intergranular corrosion known as exfoliation, which occurs in aluminum-copper alloys. The article also describes three types of erosion-corrosion: liquid erosion-corrosion, cavitation, and fretting. It concludes with information on the various factors to be considered for material selection, including minimum cost or economic design, minimum corrosion, minimum investment, and minimum maintenance.

You do not currently have access to this content.
Don't already have an account? Register

Peter Elliott, 2003. "Materials Selection for Corrosion Control", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal