Continuous Hot Dip Coatings

By
Ralph W. Leonard
Ralph W. Leonard
Coated Steels Technology, LLC
Search for other works by this author on:
Published:
2003
Page range:
786 - 793
Publication history
December 01, 2003

Abstract

This article describes the basic principles, processing steps, and benefits of continuous hot dip coatings. It provides useful information on the principal types of coatings applied in the hot-dip process. The types of coatings include galvanized coatings, galvannealed coatings, 55Al-Zn coating, 95Zn-Al coating, and aluminized coatings.

You do not currently have access to this content.
Don't already have an account? Register

Ralph W. Leonard, 2003. "Continuous Hot Dip Coatings", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal