Gaseous Corrosion-Wear Interactions

By
Joseph H. Tylczak
Joseph H. Tylczak
Albany Research Center, U.S. Department of Energy
Search for other works by this author on:
Thomas A. Adler
Thomas A. Adler
Albany Research Center, U.S. Department of Energy
Search for other works by this author on:
Published:
2003
Page range:
338 - 344
Publication history
December 01, 2003

Abstract

This article provides a discussion on the mechanisms of wear and their interactions with gaseous corrosion. The wear mechanisms include abrasive, erosive, fretting, and sliding. The measurement of degradation on combustion walls in coal-fired boilers is discussed. The article concludes with information on the common coating techniques used for wear-corrosion control.

You do not currently have access to this content.
Don't already have an account? Register

Joseph H. Tylczak, Thomas A. Adler, 2003. "Gaseous Corrosion-Wear Interactions", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal