Skip to Main Content
ASM Handbook

Corrosion: Fundamentals, Testing, and Protection

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter

Corrosion Inhibitors in the Water Treatment Industry

By
Bennett P. Boffardi
Bennett P. Boffardi
Bennett P. Boffardi and Associates, Inc.
Search for other works by this author on:
Published:
2003
Page range:
891 - 906
Publication history
December 01, 2003

Abstract

The corrosion process that occurs in industrial systems is often difficult to discern until extensive deterioration has occurred. For boilers to function properly, the incoming water must be processed to meet the water quality required for the boiler. This article discusses pretreatment methods of the incoming water and preboiler corrosion protection methods. It analyzes internal treatment and condensate treatment of boilers. The article discusses three types of cooling systems: once-through systems, open recirculating systems, and closed recirculating systems. The corrosion processes which occur in water-recirculating systems and the effect of dissolved gases, temperature, pH, suspended solids, dissolved salts, and scale deposition on corrosivity of water, are also reviewed. The article also considers anodic and cathodic inhibitors and the control of corrosion in municipal water systems.

You do not currently have access to this content.
Don't already have an account? Register

Bennett P. Boffardi, 2003. "Corrosion Inhibitors in the Water Treatment Industry", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.