Skip to Main Content
ASM Handbook

Corrosion: Fundamentals, Testing, and Protection

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter

Aqueous Corrosion-Wear Interactions

By
Iwao Iwasaki
Iwao Iwasaki
University of Minnesota Duluth
Search for other works by this author on:
Published:
2003
Page range:
331 - 337
Publication history
December 01, 2003

Abstract

This article describes the methods of wear measurements and a model of corrosive wear in mill atmospheres. It explains the polarization curves of pyrrhotite and high-carbon low-alloy steel in a quartzite slurry with examples. The surfaces of pyrrhotite in contact with mild steel or stainless steel affected by galvanic interaction are discussed. The article contains a table that lists the results of laboratory marked ball wear tests for three types of steel balls in wet grinding of magnetic taconite. It also provides information on the mechanism of electrochemical interaction and relative significance of corrosion and abrasion in wear. Galvanic interactions in multielectrode systems are reviewed. The article presents a case history on the material selection for grinding balls to minimize corrosion loss and the adverse effect on flotation.

You do not currently have access to this content.
Don't already have an account? Register

Iwao Iwasaki, 2003. "Aqueous Corrosion-Wear Interactions", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal