Skip to Main Content
ASM Handbook

Corrosion: Fundamentals, Testing, and Protection

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter

Evaluating Galvanic Corrosion

By
Harvey P. Hack
Harvey P. Hack
Northrop Grumman Corporation
Search for other works by this author on:
Published:
2003
Page range:
562 - 567
Publication history
December 01, 2003

Abstract

Galvanic corrosion, although listed as one of the forms of corrosion, is considered as a type of corrosion mechanism that is evaluated by modifying the tests used for conventional forms of corrosion. This article focuses on component testing, computer and physical scale modeling, and laboratory testing methods of evaluating galvanic corrosion. The laboratory tests fall into two categories, namely, electrochemical tests and specimen exposures.

You do not currently have access to this content.
Don't already have an account? Register

Harvey P. Hack, 2003. "Evaluating Galvanic Corrosion", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal