Aqueous Corrosion Reaction Mechanisms

By
François Huet
François Huet
Université Pierre et Marie Curie and UPR 15 of CNRS, “Laboratoire Interfaces et Systèmes Electrochimiques,” Université Pierre et Marie Curie
Search for other works by this author on:
Ricardo P. Nogueira
Ricardo P. Nogueira
Université Pierre et Marie Curie and UPR 15 of CNRS, “Laboratoire Interfaces et Systèmes Electrochimiques,” Université Pierre et Marie Curie
Search for other works by this author on:
Bernard Normand
Bernard Normand
Université Pierre et Marie Curie and UPR 15 of CNRS, “Laboratoire Interfaces et Systèmes Electrochimiques,” Université Pierre et Marie Curie
Search for other works by this author on:
Hisasi Takenouti
Hisasi Takenouti
Université Pierre et Marie Curie and UPR 15 of CNRS, “Laboratoire Interfaces et Systèmes Electrochimiques,” Université Pierre et Marie Curie
Search for other works by this author on:
Published:
2003
Page range:
52 - 60
Publication history
December 01, 2003

Abstract

Corrosion of metallic materials is governed by electrochemical kinetics, so that the general concepts developed for studying electrochemical reaction mechanisms may be applied to corrosion. This article presents the fundamental aspects of electrode kinetics. The processes of charge transfer taking place at the electrode interface within the double layer and of mass transport at the vicinity of the electrode surface are discussed. The article describes the corrosion processes, which involve anodic and cathodic reactions at specific electrode sites. Some experimental methods for devising a reliable reaction model are detailed. The article explains some reaction mechanisms for cathodic and anodic processes to illustrate the great variety of reaction mechanisms occurring at the electrode interface.

You do not currently have access to this content.
Don't already have an account? Register

François Huet, Ricardo P. Nogueira, Bernard Normand, Hisasi Takenouti, 2003. "Aqueous Corrosion Reaction Mechanisms", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal