Evaluating Pitting Corrosion

By
Bopinder Phull
Bopinder Phull
Revising author
Consultant
Search for other works by this author on:
Published:
2003
Page range:
545 - 548
Publication history
December 01, 2003

Abstract

Pitting is a form of localized corrosion that is often a concern in applications involving passivating metals and alloys in aggressive environments. This article describes the test methods for pitting corrosion. These methods include ASTM G 48, ASTM F 746, ASTM G 61, ASTM G 100, and electrochemical noise measurements. The visual examination, metallographic examination, and nondestructive inspection of pits are discussed. The article reviews the procedures for the use of standard charts, metal penetration, statistical analysis, and loss in mechanical properties to quantify the severity of pitting damage.

You do not currently have access to this content.
Don't already have an account? Register

Bopinder Phull, 2003. "Evaluating Pitting Corrosion", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.