Corrosion Monitoring Using Microwave and Guided Wave Nondestructive Evaluation

By
Alan V. Bray
Alan V. Bray
Systems and Materials Research Consultancy (SMRC)
Search for other works by this author on:
Published:
2003
Page range:
529 - 532
Publication history
December 01, 2003

Abstract

Microwave and guided wave (GW) nondestructive evaluation (NDE) techniques are capable of detecting corrosion damage, cracks, and other defect types in inaccessible areas. This article describes the operation principles of the techniques and provides information on hidden corrosion detection and the applications of microwave NDE devices and GW ultrasonic NDE devices.

You do not currently have access to this content.
Don't already have an account? Register

Alan V. Bray, 2003. "Corrosion Monitoring Using Microwave and Guided Wave Nondestructive Evaluation", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal