Skip to Main Content
ASM Handbook

Corrosion: Fundamentals, Testing, and Protection

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter

Infrared Imaging for Corrosion, Disbondments, and Cracks

By
Ignacio Perez
Ignacio Perez
Office of Naval Research
Search for other works by this author on:
Published:
2003
Page range:
525 - 528
Publication history
December 01, 2003

Abstract

This article begins with an overview of the various aspects of infrared pulse thermography used to detect disbondments, delaminations, and generalized corrosion. It describes the distinctive phases of the pulse thermographic process and the key components that are required to perform active thermography. The components include an excitation source, a thermographic camera, and a computer with software that controls the instrumentation, acquires data, and displays the results. The article discusses the process and experimental setup of sonic thermography used for crack detection.

You do not currently have access to this content.
Don't already have an account? Register

Ignacio Perez, 2003. "Infrared Imaging for Corrosion, Disbondments, and Cracks", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal