Solid Metal Induced Embrittlement

By
David G. Kolman
David G. Kolman
Revising author
Los Alamos National Laboratory
Search for other works by this author on:
Published:
2003
Page range:
393 - 397
Publication history
December 01, 2003

Abstract

Embrittlement that occurs below the melting point of the embrittling species is known as solid metal induced embrittlement (SMIE) of metals. This article provides a discussion on the characteristics and investigations of SMIE, liquid metal induced embrittlement, and delayed failure. It also describes the mechanism of SMIE.

You do not currently have access to this content.
Don't already have an account? Register

David G. Kolman, 2003. "Solid Metal Induced Embrittlement", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal