Skip to Main Content
ASM Handbook

Corrosion: Fundamentals, Testing, and Protection

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter

Anodic Protection

By
Carl E. Locke, Jr.
Carl E. Locke, Jr.
University of Kansas
Search for other works by this author on:
Published:
2003
Page range:
851 - 854
Publication history
December 01, 2003

Abstract

This article presents a brief history and the uses of the anodic protection technique. It compares anodic and cathodic protection and describes the design considerations of the anodic protection system. The article discusses the specific requirements of equipment required for anodic protection. It also explains the applications and economic aspects of anodic protection, with examples.

You do not currently have access to this content.
Don't already have an account? Register

Carl E. Locke, Jr., 2003. "Anodic Protection", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal