Book Chapter

Geochemical Modeling

By
Steven A. Matthes
Steven A. Matthes
U.S. Department of Energy, Albany Research Center
Search for other works by this author on:
Published:
2003
Page range:
34 - 41
Publication history
December 01, 2003

Abstract

Geochemical modeling is being used to understand and predict scaling, susceptibility to corrosion, atmospheric corrosion rates, acid rain, corrosion film solubility, and environmental impacts of aqueous species in runoff. This article discusses the principles, limitations, and applications of the modeling. It explains how to calculate the chemical equilibrium in geochemical modeling and provides information on modeling features.

You do not currently have access to this content.
Don't already have an account? Register

Steven A. Matthes, 2003. "Geochemical Modeling", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.