Corrosion of Carbon Steel Weldments

By
Stuart Bond
Stuart Bond
Revising author
TWI Ltd.
,
United Kingdom
Search for other works by this author on:
Published:
2003
Page range:
294 - 300
Publication history
December 01, 2003

Abstract

Corrosion of carbon steel weldments can be due to metallurgical effects, such as preferential corrosion of the heat-affected zone (HAZ) or weld metal, or it can be associated with geometrical aspects, such as stress concentration at the weld toe, or creation of crevices due to joint design. This article describes the issues related to corrosion of carbon steel weldments and the remedial measures that have proven to be successful in specific cases. It provides useful information on preferential HAZ corrosion, preferential weld metal corrosion, and galvanic corrosion.

You do not currently have access to this content.
Don't already have an account? Register

Stuart Bond, 2003. "Corrosion of Carbon Steel Weldments", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.