Rubber Coatings and Linings

By
E. Bud Senkowski
E. Bud Senkowski
KTA-Tator, Inc.
Search for other works by this author on:
Kenneth B. Tator
Kenneth B. Tator
KTA-Tator, Inc.
Search for other works by this author on:
Published:
2003
Page range:
845 - 850
Publication history
December 01, 2003

Abstract

This article presents a detailed discussion on the relative performance properties of principal rubber types used in lining applications together with their application, vulcanization and inspection techniques, and material and installation costs.

You do not currently have access to this content.
Don't already have an account? Register

E. Bud Senkowski, Kenneth B. Tator, 2003. "Rubber Coatings and Linings", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal