Corrosion Monitoring Techniques

By
P.R. Roberge
P.R. Roberge
Royal Military College of Canada
Search for other works by this author on:
R.D. Klassen
R.D. Klassen
Royal Military College of Canada
Search for other works by this author on:
Published:
2003
Page range:
514 - 518
Publication history
December 01, 2003

Abstract

Corrosion monitoring is important in the operation of modern industrial plants and in the use and maintenance of expensive assets such as bridges and aircrafts, because the damage caused by corrosion and the rate of the deterioration can be huge and the risks devastating. This article discusses the system considerations and installation techniques of different types of direct and indirect techniques in electrochemically based on-line corrosion monitoring process. It describes the importance of probe location and on-line corrosion monitoring techniques with examples.

You do not currently have access to this content.
Don't already have an account? Register

P.R. Roberge, R.D. Klassen, 2003. "Corrosion Monitoring Techniques", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal