Direct Costs of Corrosion in the United States

By
Gerhardus H. Koch
Gerhardus H. Koch
CC Technologies Laboratories, Inc.
Search for other works by this author on:
Michiel P.H. Brongers
Michiel P.H. Brongers
CC Technologies Laboratories, Inc.
Search for other works by this author on:
Neil G. Thompson
Neil G. Thompson
CC Technologies Laboratories, Inc.
Search for other works by this author on:
Y. Paul Virmani
Y. Paul Virmani
Federal Highway Administration, Turner-Fairbank Highway Research Center
Search for other works by this author on:
Joe H. Payer
Joe H. Payer
Case Western Reserve University
Search for other works by this author on:
Published:
2003
Page range:
959 - 967
Publication history
December 01, 2003

Abstract

This article first describes the two methods used in the 1998 U.S. corrosion cost study. In the first method, the cost was determined by summing the costs for corrosion control methods and contract services. In the second, the cost of corrosion was first determined for specific industry sectors and then extrapolated to calculate a national total corrosion cost. The article then reports the results and conclusions of the study. It concludes with information on corrosion prevention strategies.

You do not currently have access to this content.
Don't already have an account? Register

Gerhardus H. Koch, Michiel P.H. Brongers, Neil G. Thompson, Y. Paul Virmani, Joe H. Payer, 2003. "Direct Costs of Corrosion in the United States", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal