In-Service Techniques—Damage Detection and Monitoring

By
Vinod S. Agarwala
Vinod S. Agarwala
Revising author
Naval Air Systems Command
Search for other works by this author on:
Published:
2003
Page range:
501 - 508
Publication history
December 01, 2003

Abstract

This article focuses on the methods that are being developed for detecting and monitoring corrosion: electrochemical methods, electromagnetic or sound wave methods, fiber-optic technology, fluorescence methods, and the Diffracto Sight method. It reviews the importance of data management and the Corrosion Expert System. It concludes with information on the simulation and modeling for incorporating the mechanisms of corrosion prevention into military hardware systems design and operation.

You do not currently have access to this content.
Don't already have an account? Register

Vinod S. Agarwala, 2003. "In-Service Techniques—Damage Detection and Monitoring", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal