Skip to Main Content
ASM Handbook

Corrosion: Fundamentals, Testing, and Protection

Edited by
Stephen D. Cramer
Stephen D. Cramer
Search for other works by this author on:
Bernard S. Covino, Jr.
Bernard S. Covino, Jr.
Search for other works by this author on:
ASM International
Volume
13A
ISBN electronic:
978-1-62708-182-5
Publication date:
2003
Book Chapter

Methods for Measuring Gaseous Corrosion Rates

By
Aleksander Gil
Aleksander Gil
University of Mining and Metallurgy
,
Cracow
,
Poland
Search for other works by this author on:
Published:
2003
Page range:
115 - 116
Publication history
December 01, 2003

Abstract

This article discusses two methods for measuring gaseous corrosion rates: the discontinuous method and the continuous method. It informs that corrosion rate data can be obtained indirectly by measuring the scale thickness, scale weight per unit surface area, loss of metal thickness, loss of material weight per unit surface area, and weight change of oxidant bonded in the scale per unit surface area as a function of time, in a discontinuous manner. The continuous methods discussed include the volumetric method, the manometric method, and the thermogravimetric analysis.

You do not currently have access to this content.
Don't already have an account? Register

Aleksander Gil, 2003. "Methods for Measuring Gaseous Corrosion Rates", Corrosion: Fundamentals, Testing, and Protection, Stephen D. Cramer, Bernard S. Covino, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal