Matrix Microstructure Analysis of Fiber-Reinforced Composites[1]

By
Brian S. Hayes
Brian S. Hayes
Search for other works by this author on:
;
Luther M. Gammon
Luther M. Gammon
Search for other works by this author on:
Published:
2004
Publication history
February 26, 2011

Abstract

Microstructural analysis of the composite matrix is necessary to understand the performance of the part and its long-term durability. This article focuses on the microstructural analysis of engineering thermoplastic-matrix composites and the influence of cooling rate and nucleation on the formation of spherulites in high-temperature thermoplastic-matrix carbon-fiber-reinforced composites. It also describes the microstructural analysis of a bio-based thermosetting-matrix natural fiber composite system.

You do not currently have access to this content.
Don't already have an account? Register

Brian S. Hayes, Luther M. Gammon, 2004. "Matrix Microstructure Analysis of Fiber-Reinforced Composites", Metallography and Microstructures, George F. Vander Voort

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal